GH2132 (GH132)
Approximate brands:
GB/T | UNS | Trademark | JIS | W.Nr |
GH2132 | N66286 | IncoloyA-286 | SUH660 | 1.4980 |
Chemical constituents of GH2132:
alloy Brand | % | Ni | Cr | Mo | B | P | Al | Ti | C | Mn | Si | V | S | Fe |
GH2132 | min | 24 | 13.5 | 1.0 | 0.001 | 1.75 | 0.10 | allowance | ||||||
max | 27 | 16 | 1.5 | 0.01 | 0.03 | 0.40 | 2.35 | 0.08 | 2.0 | 1.0 | 0.50 | 0.02 |
Physical properties of GH2132:
density | 7.93 g/cm³ |
Melting point | 1364℃-1424℃ |
Minimum mechanical properties of GH2132 at room temperature:
state | TensileRm N/mm² | Yield Strength Rp 0.2N/mm² | ElongatSion A5% | Brinell HB |
Solution treatment | 610 | 270 | 30 | ≤321 |
The main characteristics of GH2132 are as follows:
It is a kind of alloy material with high strength at high temperature and resistance to oxidation at high temperature.
It has high yield strength, durability and creep strength below 650 C, and has good processing plasticity and satisfactory weldability.
GH2132 applications:
Used for turbine disc, annular body, stamping and welding parts, fastening parts materials under 700 degree C.
Widely used in the manufacture of aeroengine and industrial gas turbine components, such as turbine blades,
Afterburner is also widely used in automotive engines.